RTM is a closed-mold process used to manufacture fiber-reinforced composite parts. During production, dry fiber reinforcement is placed inside a mold. Liquid resin is then injected into the cavity under pressure to impregnate the fiber preform.
If resin flow is restricted or filling rates vary significantly across the mold, defects such as dry spots, voids, incomplete impregnation, and resin-rich areas may occur. These problems are commonly associated with reinforcement permeability, resin properties, injection parameters, and mold design.
The structure of the reinforcement directly affects resin flow. Under otherwise similar conditions, a higher fiber volume fraction and narrower pore channels generally reduce preform permeability, increasing resistance to resin flow.
If fiber arrangement, layup orientation, or compaction varies across the preform, resin may preferentially flow through areas with lower resistance, leaving other regions inadequately impregnated. When multiple reinforcement materials are combined, differences in permeability between layers must also be considered.
▸ Closed Mold Mat CF consists of a synthetic nonwoven core with chopped glass fibers laminated on both sides. It can be used in RTM and other closed-mold processes. Selecting a suitable material structure and layup can help improve resin flow and thickness consistency, although the actual results depend on the molding conditions.
Resin viscosity affects how easily resin flows through the gaps between fibers. Excessively high viscosity increases flow resistance and may extend mold filling time. If the resin begins to gel before filling is complete, its flowability gradually decreases, making it difficult to impregnate unfilled areas.
Resin temperature, mixing ratio, and working time should therefore be controlled according to the resin system to maintain suitable flow characteristics during injection.
Injection pressure and flow rate must be matched to reinforcement permeability and resin viscosity. Insufficient pressure may slow mold filling and increase the risk of premature gelation. Excessive pressure or flow rate, however, may cause the fiber preform to shift, deform, or become locally compacted, changing the intended resin flow paths.
Simply increasing injection pressure is not a reliable solution to poor impregnation. Process settings should be determined according to mold dimensions, reinforcement structure, and the resin's processing window.
The position and number of injection gates influence resin flow direction. Poor gate placement may cause some areas to fill before others are adequately impregnated.
Vent design is equally important. When resin flow fronts from different directions meet, trapped air may remain inside the reinforcement if it cannot escape through the vents. This can lead to voids or localized dry spots.
In addition, excessive gaps between the reinforcement and mold surface may allow resin to flow rapidly along low-resistance paths, bypassing parts of the fiber preform. This phenomenon is known as race tracking and can result in incomplete internal impregnation.
⚑ Dry spots and voids should be distinguished during troubleshooting. A dry spot is an area where the reinforcement has not been adequately impregnated with resin, while a void is an air or gas-filled space trapped inside the finished part. Both defects may occur together, but they require different inspection approaches.